Thermal Properties Metric English Comments
Specific Heat Capacity 0.980 J/g-°C

@Temperature -70.0 °C
0.234 BTU/lb-°F

@Temperature -94.0 °F
3M Novec™ 7500 Engineered Fluid
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a..