Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.934 J/g-°C @Temperature 700 °C |
0.223 BTU/lb-°F @Temperature 1290 °F |
|
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |
|||
Specific Heat Capacity | 0.935 J/g-°C @Temperature 200 °C |
0.223 BTU/lb-°F @Temperature 392 °F |
|
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |