Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.616 J/g-°C @Temperature 500 °C |
0.147 BTU/lb-°F @Temperature 932 °F |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |
|||
Specific Heat Capacity | 0.615 J/g-°C @Temperature 400 °C |
0.147 BTU/lb-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |