Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.427 J/g-°C

@Temperature 100 °C
0.102 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.427 J/g-°C

@Temperature 100 °C
0.102 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Specific Heat Capacity 0.427 J/g-°C

@Temperature 100 °C
0.102 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.427 J/g-°C

@Temperature 100 °C
0.102 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Specific Heat Capacity 0.428 J/g-°C

@Temperature 25.0 °C
0.102 BTU/lb-°F

@Temperature 77.0 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..