Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.413 J/g-°C @Temperature 25.0 °C |
0.0987 BTU/lb-°F @Temperature 77.0 °F |
|
International Mold Steel Daido DRM1 Matrix High-Speed Steel This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its .. |