Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 37.7 J/g @Temperature 200 °C |
16.2 BTU/lb @Temperature 392 °F |
|
Solvay Specialty Polymers FOMBLIN® Y H-VAC 18/8 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |