Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® Y H-VAC 18/8 PFPE Pump Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y H-VAC 18/8 PFPE Pump Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and oxygen atoms, the PFPEs have exceptional properties such as: low vapor pressure; chemical inertness; non-flammability; high thermal stability; no flash or fire point; low toxicity; excellent compatibility with metals, plastics, elastomers; low volatility; good aqueous and non-aqueous solvent resistance; high dielectric properties; low surface tension; good radiation stability; and environmentally friendly-do not damage the ozone.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
ASTM D891
Kinematic Viscosity 190 cSt

@Temperature 20.0 °C
190 cSt

@Temperature 68.0 °F
ASTM D445
Molecular Weight 2800 g/mol
2800 g/mol
Vapor Pressure 2.67e-11 bar

@Temperature 20.0 °C
2.00e-8 torr

@Temperature 68.0 °F
Knudsen
2.67e-7 bar

@Temperature 100 °C
0.000200 torr

@Temperature 212 °F
Knudsen
Thermal Properties Metric English Comments
Heat of Vaporization 37.7 J/g

@Temperature 200 °C
16.2 BTU/lb

@Temperature 392 °F
Pour Point -42.0 °C
-43.6 °F
ASTM D97
Optical Properties Metric English Comments
Refractive Index 1.299
1.299
n<sub>0</sub><sup>20</sup>
Users viewing this material also viewed the following: