Thermal Properties Metric English Comments
Heat of Vaporization 159 J/g
68.4 BTU/lb
at Boiling Point
Solvay Specialty Polymers Meforex® 125 Ozone-Friendly CFC Replacement
Formula: CHF2CF3; Name: Pentafluoroethane. Replaces R 502, R22. Refrigerant blends components for low and middle temperatures.Information provided by Solvay Solexis, Inc.