Solvay Specialty Polymers Meforex® 125 Ozone-Friendly CFC Replacement

Category Fluid
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Meforex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Meforex® 125 Ozone-Friendly CFC Replacement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: CHF2CF3; Name: Pentafluoroethane. Replaces R 502, R22. Refrigerant blends components for low and middle temperatures.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc

@Temperature 25.0 °C
0.0430 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 120 g/mol
120 g/mol
Vapor Pressure 13.8 bar

@Temperature 25.0 °C
10400 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 159 J/g
68.4 BTU/lb
at Boiling Point
Melting Point -103 °C
-153 °F
at 1.013 bar
Boiling Point -48.5 °C
-55.3 °F
at 1.013 bar
Chemical Properties Metric English Comments
Critical Pressure 36.39 bar
27290 torr
Critical Temperature 66.3 °C
151 °F
Critical Density 0.570 g/cc
0.0206 lb/in³
Descriptive Properties Value Comments
Flammability Range (vol%) None
Ozone Depletion Potential 0
Based on CFC11 = 1.0
Toxicity Level 1000 ppm
Allowed limit in work places (values suggested by producers).