Heat of Vaporization 101.7 J/g
43.75 BTU/lb
3M Novec™ 7300 Engineered Fluid
3M™ Novec™ 7300 fluid is a clear, colorless, odorless fluid that has utility in a wide variety of applications, including heat transfer, lubricant deposition, electronic testing and cleaning appli..
Heat of Vaporization 101.7 J/g
43.75 BTU/lb
3M Novec™ 7300DL Engineered Fluid
3M™ Novec™ 7300DL fluid is a clear, colorless, odorless fluid. A high-purity version of 3M™ Novec™ 7300 fluid, designed for demanding applications such as hard disk lubricant deposition & semico..