Material Notes:
3M™ Novec™ 7300 fluid is a clear, colorless, odorless fluid that has utility in a wide variety of applications, including heat transfer, lubricant deposition, electronic testing and cleaning applications.Feature and Benefits:Non-flammable Zero Ozone Depletion Potential (ODP)Low toxicityExcellent materials compatibilityLow Global Warming Potential (GWP) VOC-exempt solvent (US EPA)Clear, colorless, odorless fluidInformation provided by 3M
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
Liquid
Viscosity Measure 0.71 cSt
0.71 cSt
3.51 cSt

@Temperature -35.0 °C
3.51 cSt

@Temperature -31.0 °F
Molecular Weight 350 g/mol
350 g/mol
Vapor Pressure 0.0599 bar
44.9 torr
Surface Tension 15 dynes/cm
15 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 101.7 J/g
43.75 BTU/lb
Boiling Point 98.0 °C

@Pressure 0.101 MPa
208 °F

@Pressure 14.7 psi
Descriptive Properties Value Comments
Solubility 586 ppb
of Solvent in Water
67 ppm
of Water in Solvent