Thermal Properties Metric English Comments
Heat Distortion Temperature 42.2 °C
108 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..