Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 129 °C | 264 °F | ASTM D648 |
Kotec Carbotex K-20MRA30 Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesIn.. |
|||
Heat Distortion Temperature | 129 °C | 264 °F | ASTM D648 |
Kotec Carbotex K-20T30 Polycarbonate, General Purpose Features: Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation prov.. |
|||
Heat Distortion Temperature | 129 °C | 264 °F | ASTM D648 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Heat Distortion Temperature | 129 °C | 264 °F | ASTM D648 |
Kotec Carbotex K-20UVR30 Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household ap.. |
|||
Heat Distortion Temperature | 129 °C | 264 °F | ASTM D648 |
IRPC Polimaxx Polene 1111R Polypropylene Homopolymer CHARACTERISTICS: EXCELLENT HIGH STIFFNESS, HEAT STABILITY, HIGH FLOW CONTAIN LONG TERM HEAT AGING ADDITIVE APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, COFFEE MAKER, HAIR DRYER |