Polymer Property : Heat Distortion Temperature = 257 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 125 °C
257 °F
GB1634
Beijing Evergrow Resources Oilon
Information provided by Beijing Evergrow Resources.
Heat Distortion Temperature 125 °C
257 °F
GB1634
Beijing Evergrow Resources MC Nylon
Information provided by Beijing Evergrow Resources.