Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 125 °C | 257 °F | GB1634 |
Beijing Evergrow Resources Oilon Information provided by Beijing Evergrow Resources. |
|||
Heat Distortion Temperature | 125 °C | 257 °F | GB1634 |
Beijing Evergrow Resources MC Nylon Information provided by Beijing Evergrow Resources. |