Thermal Properties Metric English Comments
Heat Distortion Temperature 95.41 °C
203.7 °F
ISO 75 A/B
Tisan TISSAN® UNR Styrene Acrylonitrile
Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy..