Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tisan TISSAN® UNR Styrene Acrylonitrile

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer Tisan Engineering Plastics
Trade Name TISSAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISSAN® UNR Styrene Acrylonitrile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy to processReasonable priceApplications:Little household equipmentsOffice equipmentsDashing componentsAutomotive instrument partsCalculator parts
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ISO 868
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2
Elongation at Yield 30 %
30 %
ISO 527
Flexural Strength 280 MPa
40600 psi
ISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
ISO 180/A
Thermal Properties Metric English Comments
Melting Point <= 118 °C
<= 244 °F
Vicat Softening Point 103.6 °C
218.5 °F
ISO 306
Heat Distortion Temperature 95.41 °C
203.7 °F
ISO 75 A/B
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: