Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 130 °C | 266 °F | ISO 75-2 |
Tisan TISMOSET® Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti.. |
|||
Heat Distortion Temperature | 130 °C | 266 °F | ISO 75-2 |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Heat Distortion Temperature | 130 °C | 266 °F | ISO 75-2 |
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Heat Distortion Temperature | 130 °C | 266 °F | ISO 75-2 |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |