Material Notes:
Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorptionEasy processingReasonable pricesApplication: Can be substituted with thermoplastics in numerous applications including the electric industry, house appliances, bath, and kitchen applications.
Physical Properties Metric English Comments
Density 1.475 - 1.49 g/cc
0.05329 - 0.0538 lb/in³
ISO 1183
Apparent Bulk Density 0.600 - 0.620 g/cc
0.0217 - 0.0224 lb/in³
ISO 60
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.75 - 2.95 kJ/m²
1.31 - 1.40 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 5.50 - 5.55 kJ/m²
2.62 - 2.64 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Heat Distortion Temperature 130 °C
266 °F
ISO 75-2
Flammability, UL94 V-0
V-0