Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 52.8 °C | 127 °F | |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |
|||
Heat Distortion Temperature | 52.8 °C | 127 °F | |
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |