BCC Products BC 7062-3H Epoxy Casting

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 7062-3H Epoxy Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yielding excessive shrinkage. Casting thicknesses may be increased by incorporating aluminum needles, puffs or granules. BC 7062, when properly cured, provides nearly perfect reproduction, resulting in a dimensionally stable, hard, tough surface. For use in constructing duplicate models, prototypes, patterns, facing dies, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.72 g/cc
1.72 g/cc
Brookfield Viscosity 3800 cP

@Temperature 23.9 °C
3800 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0027 cm/cm
0.0027 in/in
ASTM D2566-69
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 23.9 °C
85

@Temperature 75.0 °F
Tensile Strength, Ultimate 31.0 MPa
4500 psi
Flexural Strength 49.6 MPa
7200 psi
Compressive Strength 75.8 MPa
11000 psi
Thermal Properties Metric English Comments
CTE, linear 75.6 µm/m-°C
42.0 µin/in-°F
Heat Distortion Temperature 52.8 °C
127 °F
Processing Properties Metric English Comments
Cure Time >= 2880 min

@Temperature 24.0 °C
>= 48.0 hour

@Temperature 75.2 °F
Pot Life >= 240 min

@Temperature 24.0 °C
>= 240 min

@Temperature 75.2 °F
2 lb. mass
Descriptive Properties Value Comments
Machinability Excellent
Mix Ratio 6:1 by weight, 2.9:1 by volume, resin/harder