Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 85.0 - 105 °C | 185 - 221 °F | Average value: 96.4 °C Grade Count:7 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |