Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75/B |
Iran Petrochemical (PCC) EP-N31MA Polypropylene EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu.. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75/B |
Iran Petrochemical (PCC) S 30 S Polypropylene This grade is for general injection molding applications.Applications: textile bobbins ,wheels ,fittings ,closures ,caps.Information provided by Iran Petrochemical Commercial Co. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75B |
Lucite International Diakon® CMG314V Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75/B |
Iran Petrochemical (PCC) S 28 F Polypropylene Film Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial C.. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75/B |
Iran Petrochemical (PCC) S 30 G Polypropylene The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe.. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75-2 |
Tisan TISAKRIL® Flame Retardant (V0) ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75-2 |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Heat Distortion Temperature | 105 °C | 221 °F | ISO 75-2 |
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |