Material Notes:
EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furniture, toy boxes, small containers, video boxes, margarine, tubes.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 100 g/10 min
100 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ISO 868
Tensile Stress 30.0 MPa
4350 psi
ISO R527
Elongation at Yield 7.0 %
7.0 %
ISO R527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 150 °C
302 °F
ISO 306/A
Heat Distortion Temperature 105 °C
221 °F
ISO 75/B