Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature 55.0 - 160 °C
90.0 µin/in-°F

@Temperature 131 - 320 °F
ASTM E 831
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature 55.0 - 160 °C
90.0 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 162 µm/m-°C

@Temperature 55.0 - 160 °C
90.0 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® FG6129 NC010 PBT  (Unverified Data**)