Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 100 - 200 °C |
45.0 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 0.000 - 100 °C |
45.0 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 830F PBT+PET PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Europe-Africa-Middle East) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Americas regi.. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific) Multi purpose V1 grade |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
45.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 100 - 200 °C |
45.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
CTE, linear, Transverse to Flow | 81.0 µm/m-°C @Temperature 0.000 - 100 °C |
45.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |