Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature -40.0 - 40.0 °C |
77.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature -40.0 - 40.0 °C |
77.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature 55.0 - 160 °C |
77.2 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature 55.0 - 160 °C |
77.2 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature 55.0 - 160 °C |
77.2 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 139 µm/m-°C @Temperature 55.0 - 160 °C |
77.2 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |