CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature -40.0 - 40.0 °C
77.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature -40.0 - 40.0 °C
77.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 55.0 - 160 °C
77.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 55.0 - 160 °C
77.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 55.0 - 160 °C
77.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 55.0 - 160 °C
77.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers