Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |