Polymer Property : CTE, linear, Transverse to Flow = 36.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 943X PC Copolymer
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific)
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 160 - 249 °C
36.1 µin/in-°F

@Temperature 320 - 480 °F
ASTM E228
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 100 - 200 °C
36.1 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 100 - 200 °C
36.1 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature -40.0 - 60.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 6
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 64.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
36.1 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy
Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr..
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 55.0 - 160 °C
36.1 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers