Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 60.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |