Polymer Property : CTE, linear, Transverse to Flow = 51.4 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 51.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES
LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone.
CTE, linear, Transverse to Flow 51.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific)
LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color.
CTE, linear, Transverse to Flow 51.4 µm/m-°C

@Temperature -30.0 - 80.0 °C
28.6 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 non-halogen FR compound