Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
CTE, linear, Transverse to Flow | 51.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
CTE, linear, Transverse to Flow | 51.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
CTE, linear, Transverse to Flow | 51.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
CTE, linear, Transverse to Flow | 51.4 µm/m-°C @Temperature -30.0 - 80.0 °C |
28.6 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |