Polymer Property : CTE, linear, Transverse to Flow = 40.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 73.4 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound
CTE, linear, Transverse to Flow 73.4 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated
CTE, linear, Transverse to Flow 73.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DEI13F PC
LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R..