Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 68.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Transverse to Flow | 68.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Transverse to Flow | 68.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Transverse to Flow | 68.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
CTE, linear, Transverse to Flow | 68.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |