Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 66.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Transverse to Flow | 66.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Transverse to Flow | 66.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubriloy D20001 PC LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by.. |
|||
CTE, linear, Transverse to Flow | 66.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 66.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 66.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |