Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 46.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
CTE, linear, Transverse to Flow | 46.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Transverse to Flow | 46.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX01303C PC LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |