Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 37.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX99873C PC
LNP STAT-KON* DX99872C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.