Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 270 µm/m-°C @Temperature -40.0 - 23.0 °C |
150 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |