CTE, linear, Transverse to Flow 200 µm/m-°C

@Temperature 55.0 - 160 °C
111 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers