Polymer Property : CTE, linear, Parallel to Flow = 88.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East)
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 160 - 249 °C
48.9 µin/in-°F

@Temperature 320 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X6125 PBT+PC
Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X6125 PBT+PC
Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region.