Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1162T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
CTE, linear, Parallel to Flow | 74.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |