Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 131 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC LNP* LUBRILOY* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, High Impact. |
|||
CTE, linear, Parallel to Flow | 131 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific) LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |