Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 131 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY D2000I PC
LNP* LUBRILOY* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, High Impact.
CTE, linear, Parallel to Flow 131 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific)
LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.