Polymer Property : CTE, linear, Parallel to Flow = 70.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific)
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific)
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature -40.0 - 40.0 °C
70.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific)
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.