Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific) LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 127 µm/m-°C @Temperature -40.0 - 40.0 °C |
70.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific) LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |