Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 7.00 µm/m-°C @Temperature 100 - 200 °C |
3.89 µin/in-°F @Temperature 212 - 392 °F |
2 |