Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 100 - 200 °C
3.89 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..