Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding. |
|||
CTE, linear, Parallel to Flow | 59.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific) LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding. |