Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated.
CTE, linear, Parallel to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
CTE, linear, Parallel to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.